MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese SO.F.TER Sofprene T® 5402.A60 SBS TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Injection molding grade

Sofprene T® is a thermoplastic elastomer with SBS. Applications include Furniture (shock-absorbers for bed slats, wheels, anti-shocks profiles), Household goods (anti-slip mats, handles for tools, overmolded rubber lips for dustpan and squeegees, plungers), and Toys (wheels, handles, seats, little toys).

Information provided by SO.F.TER. Spa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D 792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60ASTM D2240
Tensile Strength 4.80 MPaASTM D412 C
Elongation at Break 680 %ASTM D412-C
100% Modulus 0.00140 GPa
@Strain 100 %
ASTM D412 C
Tear Strength 25.0 kN/mASTM D624 C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese SO.F.TER Sofprene® TPU Effect 38 K SBS Foot Ware Compound
Celanese SO.F.TER Sofprene® Vulcanized Rubber 38 KH SBS Foot Ware Compound
Celanese SO.F.TER Sofprene® TPU Effect 38S SBS Foot Ware Compound

PSOFS748 / 162212

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.