Geon® Performance Solutions Vinyl Rigid Extrusion 87548 AS Polyvinyl Chloride, Rigid
Categories:
Polymer
;
Thermoplastic
;
Vinyl (PVC)
;
PVC, Rigid Grade
Material Notes:
A transparent PVC profile compound, with reduced surface resistivity, resulting in unlikely attraction and adhesion of dust. Actual results on surface resistivity = 1.3x10^15.
Geon Performance Solutions was created from PolyOne in 2019.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.33
g/cc
1.33
g/cc
ASTM D792
Mechanical Properties
Metric
English
Comments
Hardness, Shore D
82
82
15 sec; ASTM D2240
Tensile Strength, Yield
53.4
MPa
7750
psi
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus
2.79
GPa
405
ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength
88.5
MPa
12800
psi
ASTM D790
Flexural Modulus
2.84
GPa
412
ksi
ASTM D790
Izod Impact, Notched
1.40
J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
2.62
ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Flow; ASTM D256A
5.70
J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
10.7
ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
11.0
J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
20.6
ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Dart Drop Total Energy
52.0
J/cm
@Temperature 23.0 °C
0.0974
ft-lb/mil
@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
173
J/cm
@Temperature 23.0 °C
0.324
ft-lb/mil
@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
Optical Properties
Metric
English
Comments
Transmission, Visible
90 %
90 %
transparent; thickness not quantified
Processing Properties
Metric
English
Comments
Melt Temperature
182
-
193
°C
360
-
379
°F
Compliance Properties
Metric
English
Comments
FDA
Yes
Yes
Food Contact, Unspecified Rating
Descriptive Properties
Appearance
Clear/Transparent
Features
High Impact Resistance
Forms
Pellets
Generic Material
PVC, Rigid
Generic Name
Polyvinyl Chloride, Rigid (PVC, Rigid)
Processing Method
Extrusion
Regional Availability
Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses
Profiles
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PH0POL1218 / 145787
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.