MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Redwood Plastics Redco™ ACRYLIC CAST SHEET
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Cast

Material Notes:

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ASTM D792
Water Absorption 0.20 %
@Thickness 3.17 mm,
Time 86400 sec
0.20 %
@Thickness 0.125 in,
Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 100 - 102100 - 102ASTM D785
Tensile Strength 72.4 MPa10500 psiASTM D638
Elongation at Break 5.0 %5.0 %ASTM D638
Tensile Modulus 3.10 GPa450 ksiASTM D638
Flexural Strength 114 MPa16500 psiASTM D790
Flexural Modulus 3.10 GPa450 ksiASTM D790
Izod Impact, Notched 0.214 J/cm0.400 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+17 ohm-cm>= 1.00e+17 ohm-cmASTM D257
Dielectric Constant  2.5
@Frequency 1e+6 Hz
2.5
@Frequency 1e+6 Hz
ASTM D150
 3.3
@Frequency 1000 Hz
3.3
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 19.7 kV/mm
@Thickness 3.17 mm
500 kV/in
@Thickness 0.125 in
ASTM D149
Dissipation Factor  0.020 - 0.030
@Frequency 1e+6 Hz
0.020 - 0.030
@Frequency 1e+6 Hz
ASTM D150
 0.040
@Frequency 1000 Hz
0.040
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 39.0 µm/m-°C21.7 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 225 °C437 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 200 - 215 °C392 - 419 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.491.49ASTM D542
Transmission, Visible 92 %92 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREDW109 / 296675

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.