MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Pro-fax™ PH835 Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Fiber Grade

Material Notes: Description: Pro-fax™ PH835 is a very high melt flow, controlled rheology polypropylene homopolymer resin designed for spunbond and continuous filament applications that require superior spinnability and finer fibers. Pro-fax™ PH835 resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. All ingredients in Pro-fax™ PH835 resin meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Fibers

Information provided by Basell.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.902 g/cc0.0326 lb/in³ASTM D792
Melt Flow 34 g/10 min
@Load 2.16 kg,
Temperature 230 °C
34 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PPH 3925WZ Polypropylene, Injection Molding Grade
Braskem H 107 Injection Molding Polypropylene
LyondellBasell Pro-fax™ PH350 Polypropylene Homopolymer
LyondellBasell Pro-fax™ RP320N Polypropylene Copolymer
LyondellBasell Pro-fax™ SC973 Polypropylene Copolymer

PMO876 / 53865

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.