MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Aquathene FR 439800X01
Categories: Polymer; Thermoplastic

Material Notes: The Aquathene product line encompasses the Wire & Cable moisture cross-linkable system used in a variety of power cable applications; these include ethylene vinyl silane copolymers along with the complementary catalyst, flame retardant and black master batches, with applications ranging from low voltage insulations to medium voltage jacketing.

Aquathene FR439800 is a colorable flame retardant catalyst master batch selected for use in moisture cure applications. When FR439800 is melt blended with Aquathene AQ120000 in a 35% / 65% ratio, respectively, and cross linked after exposure to moisture, this formulation is typically used in low voltage power and control cable applications where UL44 specifies horizontal flame rating with 90°C service in wet locations. Applications: Wire & Cable

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.47 g/ccASTM D1505
Melt Flow 0.85 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Descriptive Properties
Processing MethodWire & Cable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Aquathene® AQ120000 Ethylene Vinylsilane Copolymer
LyondellBasell Aquathene PM 92949C
LyondellBasell Aquathene CM 04483

PEQT7073 / 218711

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.