MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Superplastic Zinc (Zn-22Al), As-Rolled - Transverse Properties
Categories: Metal; Nonferrous Metal; Zinc Alloy

Material Notes:

Properties vary with rolling direction. Average values and values for longitudinal direction are listed separately.

Key Words: Super Z300; Formetal 22 Alloy; Korloy 2684
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 5.20 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 70 - 79500 kg load; 10 mm hardened steel ball
Hardness, Knoop 98Estimated from Brinell Value
Hardness, Vickers 85Estimated from Brinell Value
Tensile Strength, Ultimate 380 MPa
Tensile Strength, Yield 297 MPa
@Strain 0.2 %
Elongation at Break 25 %in 5 cm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000600 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 21.5 µm/m-°C
@Temperature 20.0 °C
 
Processing PropertiesOriginal ValueComments
Hot-Working Temperature 250 - 270 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 21 - 23 %
Cadmium, Cd <= 0.010 %
Copper, Cu 0.40 - 0.60 %
Iron, Fe <= 0.0020 %
Lead, Pb <= 0.010 %
Magnesium, Mg 0.0080 - 0.012 %
Tin, Sn <= 0.0010 %
Zinc, Zn 76.365 - 78.592 %As balance
 
Descriptive Properties
Damping27.8 Q-1 x 103at 100 Hz, 100°C
 7.8 Q-1 x 103at 100 Hz, 20°C

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Superplastic Zinc (Zn-22Al), As-Rolled - Longitudinal Properties
Superplastic Zinc (Zn-22Al), Rolled and Annealed - Transverse Properties
Superplastic Zinc (Zn-22Al), Rolled and Annealed - Longitudinal Properties
Superplastic Zinc (Zn-22Al), Rolled and Annealed
Superplastic Zinc (Zn-22Al), As-Rolled

MZN741 / 14555

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.