MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Go Yen Chemical Goyenchem-ABS37 ABS Resin
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Characteristic:
  • High rigidity and intensity
  • Cost effective
Applications: Electronic outer covering, OA appliances and items, Clocks, household appliances, daily supplies, and material of high rigidity in 3C products

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D792
Melt Flow  2.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
2.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 20 g/10 min
@Load 10.0 kg,
Temperature 200 °C
20 g/10 min
@Load 22.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 115115ASTM D785
Tensile Strength at Break 35.3 MPa
@Thickness 3.17 mm
5120 psi
@Thickness 0.125 in
ASTM D638
Tensile Strength, Yield 42.2 MPa
@Thickness 3.17 mm
6120 psi
@Thickness 0.125 in
ASTM D638
Elongation at Break 30 %30 %ASTM D638
Flexural Yield Strength 73.5 MPa10700 psi2.8mm/min; ASTM D790
Flexural Modulus 2.55 GPa370 ksi2.8mm/min; ASTM D790
Izod Impact, Notched 1.67 J/cm3.13 ft-lb/inA method, 1/2 n×1/2 n×5/2n; ASTM D256
 1.96 J/cm3.67 ft-lb/inA method, 1/8 n×1/2 n×5/2n; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C
@Thickness 12.7 mm
181 °F
@Thickness 0.500 in
Unannealed; ASTM D648
Vicat Softening Point 103 °C
@Load 1.00 kg,
Thickness 3.17 mm
217 °F
@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN778 / 267086

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.