MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik VESTAMID® HTplus LDS3031 PA10T/X, GF10  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Characterization: 10% glass fibers, mineral reinforced, medium viscosity, stabilized, qualified for LPKF LDS process, optimized shrinkage, suitable for lead-free solders. Partly biobased and eco-friendly

Applications: Three-dimensional interconnect devices in electronic applications, specially adapted for the LDS process. Dimension-stable, glossy surface

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.56 g/cc0.0564 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 84.0 MPa12200 psiISO 527-1/2
Elongation at Break 1.1 %1.1 %ISO 527-1/2
Tensile Modulus 9.60 GPa1390 ksiISO 527-1/2
Charpy Impact Unnotched  2.00 J/cm²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 2.10 J/cm²
@Temperature 23.0 °C
9.99 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.230 J/cm²
@Temperature 23.0 °C
1.09 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 0.230 J/cm²
@Temperature -30.0 °C
1.09 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 285 °C545 °FISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 243 °C469 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 279 °C534 °FISO 75

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese VECTRA E840i LDS LCP, 40% Mineral Reinforced
Mitsubishi Xantar® LDS 3720 Polycarbonate
Evonik VESTAMID® HTplus LDS1031 PA6T/X, GF10
Mitsubishi Xantar® LDS 3730 Polycarbonate
Celanese VECTRA E845i LDS LCP, 40% Mineral / Glass Reinforced

PEVONIL266 / 196470

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.