MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Hytrel® 4056P TPC-ET
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: 40 Shore D High Performance Polyester Elastomer in Powder Form

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow  5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
cm³/10min Volumetric; ISO 1133
 5.6 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.6 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 373715s; ISO 48-4
 <= 43<= 43ISO 48-4
Tensile Stress at Strain  2.40 MPa
@Strain 5.0 %
348 psi
@Strain 5.0 %
1BA specimen at 50mm/min; ISO 527-1/-2
 4.60 MPa
@Strain 10 %
667 psi
@Strain 10 %
ISO 527-1/-2
 8.40 MPa
@Strain 50 %
1220 psi
@Strain 50 %
ISO 527-1/-2
Tensile Modulus 0.0600 GPa8.70 ksiISO 527-1/-2
Flexural Modulus 0.0640 GPa9.28 ksiISO 178
Poissons Ratio 0.500.50
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eA
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eA
Tensile Impact Strength 230 kJ/m²
@Temperature 23.0 °C
109 ft-lb/in²
@Temperature 73.4 °F
Notched; ISO 8256/1
Tensile Creep Modulus, 1 hour 54.0 MPa7830 psi1h; ISO 899-1
Tensile Creep Modulus, 1000 hours 40.0 MPa5800 psi1000h; ISO 899-1
Tear Strength 96.0 kN/m548 plinormal; ISO 34-1
 102 kN/m582 pliparallel; ISO 34-1
Abrasion 200200mm3; ISO 4649
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 152 °C306 °F10°C/min; ISO 11357-1/-3
Glass Transition Temp, Tg -50.0 °C-58.0 °F10°C/min; ISO 11357-1/-2
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
<= 3.15 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Drying Temperature 80.0 °C176 °FInjection
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.080 %<= 0.080 %Injection
 
Descriptive Properties
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Part Marking Code>TPC-ET<ISO 11469
PolymerTPC
Resin IdentificationTPC-ETISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Hytrel® 4056 TPC-ET
Celanese Hytrel® 4068 TPC-ET
Celanese Hytrel® 4069 TPC-ET
Celanese Hytrel® 4556 TPC-ET
Celanese Hytrel® 30HS PA+TPC-ET

PDSX5175 / 197815

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.