MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Alathon® L5485 High Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Applications
ALATHON L 5485 is a medium molecular weight, high density polyethylene copolymer for use in blown film applications. Typical applications include general purpose HDPE film applications such as overwrap, laminating base films, food packaging, and oriented tapes.

Regulatory Status
ALATHON L 5485 meets the requirements of Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply.

Processing Techniques
Specific recommendations for processing ALATHON L 5485 can only be made when the processing conditions, equipment and end use are known.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.954 g/ccASTM D1505
Thickness 2.00 mil
Melt Flow 0.85 g/10 min
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 3700 psiASTM D882
Film Tensile Strength at Yield, TD 3800 psiASTM D882
Film Elongation at Break, MD 700 %ASTM D882
Film Elongation at Break, TD 750 %ASTM D882
Elmendorf Tear Strength MD 32 gASTM D1922
Elmendorf Tear Strength TD 1000 gASTM D1922
Elmendorf Tear Strength, MD 16.0 g/milbased on 2 mil film; ASTM D1922
Elmendorf Tear Strength, TD 500 g/milbased on 2 mil film; ASTM D1922
Film Tensile Strength at Break, MD 7900 psiASTM D882
Film Tensile Strength at Break, TD 3400 psiASTM D882
1% Secant Modulus, MD 135000 psiASTM E111
1% Secant Modulus, TD 180000 psiASTM E111
 
Processing PropertiesOriginal ValueComments
Melt Temperature 390 - 410 °F
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Global S-5000 High Density Polyethylene
Braskem HF 0150 HDPE Blown Film Extrusion Polyethylene
SCG Chemicals EL-Lene™ H5480S High Density Polyethylene Monofilament
Kazanorgsintez PE80B-285 High Density Polyethylene Composite, Film Grade
Kazanorgsintez 293-285SK High Density Polyethylene Composite, Film Grade

PEQU0696 / 37165

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.