MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röhm ACRYLITE® LED 8N LD96 Acrylic Molding Compound  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Product Profile: ACRYLITE® LED 8N LD96 Acrylic Molding Compound is a highly transparent light guide material based on ACRYLITE® 8N. In addition to the typical properties of ACRYLITE®, such as
  • Excellent weather resistance
  • UV-stability
  • Good flow, high mechanical strength
ACRYLITE® LED 8N LD96 is developed for edge lit LED applications. The light scattering properties convert the light guide to a full illuminated panel. Furthermore, the material allows for a completely transparent view through the light guide when it is not illuminated. This opens a new degree of freedom for designers. ACRYLITE® 8N LD12 is recommended for panels with a distance of 48 cm to 96 cm between two light injecting LED strips.

Application: Injection molding or extrusion.

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccASTM D729
Water Absorption <= 0.30 %ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 in/inASTM D955
Melt Flow 3.3 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 95ASTM D785
Tensile Strength at Break 77.9 MPaASTM D638
Elongation at Break 4.0 - 6.0 %ASTM D638
Elongation at Yield 4.0 - 6.0 %ASTM D638
Tensile Modulus 3200 MPaASTM D638
Flexural Strength 111.7 MPaASTM D790
Flexural Modulus 3.50 GPaASTM D790
Izod Impact, Notched (ISO) 0.360 kJ/m²
@Thickness 6.35 mm,
Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 72.0 µin/in-°F
@Temperature 0.000 - 100 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
@Thickness 6.35 mm
ASTM D648
Vicat Softening Point 108 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze <= 1.0 %ASTM D1003
Yellow Index <= 1.0 %ASTM D1925
Transmission, Visible 92 %ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röhm Plexiglas® 8N PMMA Molding Compound
Röhm ACRYLITE® LED 8N LD12 Acrylic Molding Compound
Röhm Acrylite® 8N Acrylic Polymer
Röhm ACRYLITE® LED 8N LD24 Acrylic Molding Compound
Röhm ACRYLITE® LED 8N LD48 Acrylic Molding Compound

PEVONIL076 / 196280

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.