MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
KaMin Polyfil® WC-426 Kaolin Clay - Calcined
Categories: Ceramic; Clay; Kaolin Clay

Material Notes: Fine particle size vinyl-functional calcined clay for outstanding wet electricals and long term stability in wire and cable applications.

Industry: Rubber & Plastic

Uses: Non-Black Rubber, General Rubber Goods, EPDM, Wire & Cable

Information provided by KaMin LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.60 g/cc
Brightness 93 %Reflectance (TAPPI)
Oil Absorption 65 %
Moisture Absorption at Equilibrium <= 0.5 %As Produced
Particle Size 0.70 µmAverage Stokes Equivalent Diameter
 1.5 µmMedian (Malvern Laser)
Particle Mesh Size 325 Mesh0.01% Retained
pH 6100 g/250 ml H2O Slurry
Specific Surface Area 15 m²/gBET
 
Descriptive Properties
CAS NumberProprietary
Crystalline Silica (quartz)<0.1%
Physical FormDry
Shipping PointMacon, GA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
KaMin Polyfil® 70 Kaolin Clay - Calcined
KaMin Polyfil® 90 Kaolin Clay - Calcined
KaMin Polyfil® 80 Kaolin Clay - Calcined
KaMin Polygloss® 90 Kaolin Clay - Ultrafine, high brightness
KaMin Lithosperse® 7005CS Kaolin Clay - Surface Treated

CKAMAN946 / 178417

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.