MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Inno-Comp INNOPOL® CS 2-9120 20% Talc-Filled Polypropylene Block-Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes: INNOPOL® CS 2-9120 is a 20% talc-filled compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.

INNOPOL® CS 2-9120 is developed for producing injection molded automotive components.

All information provided by INNO-COMP.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/cc
@Temperature 23.0 °C
ISO 1183
Melt Flow 30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 25.0 MPa50 mm/min; ISO 527-1,-2
Elongation at Yield 3.0 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2100 MPa1 mm/min; ISO 527-1,-2
Flexural Modulus 2200 MPa2 mm/min; ISO 178
Charpy Impact, Notched 0.200 J/cm²
@Temperature -20.0 °C
ISO 179/1eA
 0.500 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 120 °CISO 75-1,-2
 
Descriptive Properties
ColorNatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Inno-Comp INNOPOL® CS 3-9120 SR5 17% Talc Filled Polypropylene Blend
Niche Polymer PPCT20BK Copolymer PP, 20% Talc Filled
Niche Polymer PPHT40BK Homopolymer PP, 40% Talc Fiber Filled
A. Schulman Lucent TPP-320 Polypropylene, 20% Talc Filled, Impact Modified
A. Schulman Lucent TPP-220 Polypropylene, 20% Talc Filled, Impact Modified

PINNO055 / 82716

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.