MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC Lexan® 121 PC  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small intricate parts.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Density 1.19 g/ccASTM D792
Water Absorption 0.15 %
@Time 86400 sec
ASTM D570
Moisture Absorption at Equilibrium 0.35 %ASTM D570
 0.58 %
@Temperature 100 °C
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC Method
Melt Flow 17.5 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 70ASTM D785
Hardness, Rockwell R 118ASTM D785
Tensile Strength at Break 68.0 MPaType I, 50 mm/min; ASTM D638
Tensile Strength, Yield 62.0 MPaType I, 50 mm/min; ASTM D638
Elongation at Break 125 %Type I, 50 mm/min; ASTM D638
Elongation at Yield 7.0 %Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 96.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2340 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 694 J/mASTM D256
Izod Impact, Unnotched 3204 J/mASTM D4812
Tensile Impact Strength 546 kJ/m²Type S; ASTM D1822
Dart Drop, Total Energy 62.0 JInstrumented Impact Energy @ peak; ASTM D3763
 169 JASTM D3029
Taber Abrasion, mg/1000 Cycles 10CS-17, 1 kg; ASTM D1044
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+17 ohm-cmASTM D257
Dielectric Constant 2.96
@Frequency 1e+6 Hz
ASTM D150
 3.17
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 14.9 kV/mm
@Thickness 3.20 mm
in air; ASTM D149
Dissipation Factor 0.00090
@Frequency 50.0 - 60.0 Hz
ASTM D150
 0.010
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 250 - 400 VUL 746A
Hot Wire Ignition, HWI 30 - 60 secUL 746A
High Amp Arc Ignition, HAI 60 - 120 arcsUL 746A
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 68.4 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E 831
Specific Heat Capacity 1.25 J/g-°CASTM C351
Thermal Conductivity 0.250 W/m-KASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 137 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 129 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 154 °CRate B/50; ASTM D1525
UL RTI, Electrical 130 °CUL 746B
UL RTI, Mechanical with Impact 130 °CUL 746B
UL RTI, Mechanical without Impact 130 °CUL 746B
Flammability, UL94 HB
@Thickness 0.710 mm
UL 94
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586ASTM D542
Haze 1.0 %
@Thickness 2.54 mm
ASTM D1003
Transmission, Visible 88 %2.54 mm; ASTM D1003
 
Descriptive Properties
Radiant Panel ListingYESUL Tested
Specific Volume0.83cm^3/gASTM D792
UV-light, water exposure/immersionF2UL 746C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Celcon® MC90 POM, Mineral Reinforced
Elastocon TPE Technologies Elastocon® 8058N Thermoplastic Elastomer
Free-Cutting Brass, UNS C36000
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Overview of materials for Polycarbonate, Molded

PSABI51147 / 151193

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.