MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Rogers Arlon 44426R010 0.010" Cured/Uncured Silicone Rubber Laminate with Fiberglass Substrate
Categories: Polymer; Thermoset; Silicone; Silicone, Molded, Glass Fiber Filled

Material Notes: Design/Construction:
  • Interleave: 0.003" Polyethylene
  • Side 1: Cured Silicone Rubber
  • Side 2: Uncured Silicone Rubber
  • Substrate: Prime Coated 1165 Fiberglass

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.8 microns2.00 milSide 1
 76.2 microns3.00 milSide 2
 140 microns5.50 milSubstrate
 254 microns10.0 milOverall Thickness
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5858Silicone Property
Tensile Strength >= 5.52 MPa>= 800 psiSilicone Property
Elongation at Break >= 300 %>= 300 %Silicone Property
Peel Strength >= 0.877 kN/m>= 5.00 pliBond Strength
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength >= 15.7 kV/mm>= 400 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Inert 232 °C450 °F
Minimum Service Temperature, Air -56.7 °C-70.0 °F
Flammability Test 3.03.0Inches; Char Length
 2525Seconds; Flame and Glow Time
 
Processing PropertiesMetricEnglishComments
Cure Time 120 min
@Temperature 204 °C
2.00 hour
@Temperature 400 °F
Recommended Post Cure Cycle
 15.0 min
@Pressure 0.345 MPa,
Temperature 177 °C
0.250 hour
@Pressure 50.0 psi,
Temperature 350 °F
Recommended Cure Cycle
Shelf Life 6.00 Month
@Temperature 23.9 °C
6.00 Month
@Temperature 75.0 °F
 
Descriptive Properties
ColorRed
Total Product Weight (oz/yd2)12.3
Uncoated Fabric Break Strength (lb/in)125Warp Direction, Substrate Property
 160Fill Direction, Substrate Property

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Momentive Performance Materials Silopren™ LSR 2650 ZKS Custom Liquid Silicone Rubber - Automotive
Momentive Performance Materials Silopren™ LSR 4040 Liquid Silicone Rubber - Healthcare
Momentive Performance Materials Silopren™ LSR 2660 ZKS Custom Liquid Silicone Rubber - Automotive
Momentive Performance Materials Silopren™ LSR 2650 Liquid Silicone Rubber - Fast Cure / High Tear
Momentive Performance Materials Electro 1700 Heat Cured Rubber - High Voltage Insulating

PARL9746 / 148899

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.