MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Elastamax™ XL-2075 Thermoplastic Polyolefin Elastomer (TPO (POE))  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Olefinic TPE

Material Notes: PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance of physical properties and processability, and are an economical alternative to traditional thermoset rubber and more costly thermoplastic elastomers.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 828215 sec; ASTM D2240
 8787ASTM D2240
Tensile Strength at Break 7.86 MPa1140 psi510 mm/min; ASTM D412A
Tensile Stress at Strain  4.00 MPa
@Strain 100 %
580 psi
@Strain 100 %
510 mm/min; ASTM D412A
 4.69 MPa
@Strain 300 %
680 psi
@Strain 300 %
510 mm/min; ASTM D412A
Elongation at Break 760 %760 %510 mm/min; ASTM D412A
Tear Strength 43.8 kN/m250 pliDie C, 510 mm/min; ASTM D624
Compression Set 45 %
@Temperature 23.0 °C,
Time 79200 sec
45 %
@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395B
 
Descriptive Properties
AdditiveUV Stabilizer
FeaturesGeneral Purpose
FormsPellets
Generic MaterialTPO (POE)
Generic NameThermoplastic Polyolefin Elastomer (TPO (POE))
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesConstruction Applications
 General Purpose
 Industrial Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Elastamax™ XL-2055 Thermoplastic Polyolefin Elastomer (TPO (POE))
Avient Elastamax™ XL-2155 Thermoplastic Polyolefin Elastomer (TPO (POE))
Avient Elastamax™ XL-2175 Thermoplastic Polyolefin Elastomer (TPO (POE))
Avient Elastamax™ XL-2060 Black 2001 Thermoplastic Polyolefin Elastomer (TPO (POE))
Avient Elastamax™ XL-2065 Thermoplastic Polyolefin Elastomer (TPO (POE))

PH0POL0460 / 145029

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.