MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Garlock MULTI-SWELL™ 3760 Compressed Aramid Fiber Gasketing
Categories: Polymer; Thermoset; Aramid; Rubber or Thermoset Elastomer (TSE)

Material Notes: Aramid fibers with a proprietary rubber binder.
  • Creates compressive load in light weight flanges in oil and water service
  • Twice as compressible as standard fiber gaskets
  • Seals with low load and irregular surfaces
  • Easy to cut and handle, extremely flexible
Nuclear Regulatory Commission 10CFR 50 Appendix B Certified

Information provided by Garlock Rubber Technologies

Key Words: NRC 10CFR 50
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0492 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 6.89 MPa1000 psiacross grain; ASTM F152
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength >= 15.2 kV/mm
@Temperature 121 °C,
Time 10800 sec
>= 385 kV/in
@Temperature 250 °F,
Time 3.00 hour
0.0625 in. thickness; ASTM D149
 <= 0.394 kV/mm
@Thickness 1.59 mm
<= 10.0 kV/in
@Thickness 0.0625 in
100% RH for 96 hours; ASTM D149
 <= 0.394 kV/mm
@Thickness 3.17 mm
<= 10.0 kV/in
@Thickness 0.125 in
100% RH for 96 hours; ASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C
@Pressure 3.45 MPa
400 °F
@Pressure 500 psi
Continuous
Minimum Service Temperature, Air -73.3 °C-100 °F
 
Descriptive Properties
ColorBlue/Off-White
Compressibility, %15-30ASTM F36
Creep Relaxation, %30ASTM F38
Sealability ASTM F37B, ml/hr0.15ASTM Fuel A
 0.2Nitrogen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont™ Nomex® N102 Texturized Filament Yarn
DuPont™ Nomex® N104 Dyeable Filament Yarn
DuPont™ Nomex® 430 1600 Denier Aramid Yarn
DuPont™ Nomex® 430 1200 Denier Aramid Yarn
DuPont™ Nomex® 462 (NOMEX IIIA) Aramid Staple Fiber

PGARL832 / 157510

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.