MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® L2124 BK 9.7507 Nylon 12, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: VESTAMID® L2124 BK 9.7507 is a plasticized, heat- and light- stabilized polyamide 12 compound for the extrusion of flexible tubing and hoses especially for oil and petrochemical applications. Tubing according to DIN 73 378, Type: PA 12-PHL. Properties of compounds based on PA 12 vary little with changing humidity due to low moisture absorption. Parts made of this semi-crystalline material are characterized by exceptional impact strength, low coefficient of friction and good chemical resistance. VESTAMID® L2124 BK 9.7507 is characterized by a high melt viscosity and good dimensional control during pipe extrusion. VESTAMID® L2124 BK 9.7507 is supplied as cylindrical granules, ready for processing, in moisture-proof bags. Pigmentation may affect values. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Industrial Sector: Automotive and Mobility, Sustainable, Industry and Engineering
Sustainability: Sustainable electricity
Processing: Injection molding, Extrusion
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability), UV / light / weathering, Oil / fuels
Electrical: Insulating
Conformity: Automotive
Additives: Lubricant, Unfilled
Processing: Profile extrusion, Pipe/Tube extrusion
Special Characteristics: Semi-crystalline, Light-stabilized, U.V. stabilized, High heat resistant
Features: Low coefficient of friction
Color: Black
Additives: Plasticizer, Light stabilizer, Heat stabilizer, Processing aids
Chemical Resistance: Oil resistance, General chemical resistance

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/ccISO 1183
Water Absorption 1.30 %Sim to ISO 62
Moisture Absorption 0.500 %Sim to ISO 62
Linear Mold Shrinkage, Flow 0.00700 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0130 cm/cmISO 294-4, 2577
Melt Flow 9.00 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 42.0 MPaISO 527
Tensile Strength 28.0 MPaISO 527
Tensile Stress 28.0 MPa
@Strain 50.0 %
ISO 527
 9.00 MPa
@Strain 10.0 %,
Temperature 120 °C
 10.0 MPa
@Strain 10.0 %,
Temperature 100 °C
 10.0 MPa
@Strain 50.0 %,
Temperature 120 °C
 13.0 MPa
@Strain 10.0 %,
Temperature 80.0 °C
 15.0 MPa
@Strain 10.0 %,
Temperature 60.0 °C
 15.0 MPa
@Strain 50.0 %,
Temperature 100 °C
 17.0 MPa
@Strain 50.0 %,
Temperature 80.0 °C
 20.0 MPa
@Strain 9.00 %,
Temperature 23.0 °C
 20.0 MPa
@Strain 15.0 %,
Temperature 40.0 °C
 20.0 MPa
@Strain 50.0 %,
Temperature 60.0 °C
 20.0 MPa
@Strain 1.00 %,
Temperature -40.0 °C
Yield
 20.0 MPa
@Strain 2.00 %,
Temperature -20.0 °C
Yield
 20.0 MPa
@Strain 4.00 %,
Temperature 0.000 °C
Yield
 23.0 MPa
@Strain 50.0 %,
Temperature 40.0 °C
 25.0 MPa
@Strain 50.0 %,
Temperature 23.0 °C
 35.0 MPa
@Strain 25.0 %,
Temperature 0.000 °C
Yield
 50.0 MPa
@Strain 20.0 %,
Temperature -20.0 °C
Yield
 65.0 MPa
@Strain 10.0 %,
Temperature -40.0 °C
Yield
Tensile Strength, Yield 28.0 MPaISO 527
Elongation at Break 210 %Nominal; ISO 527
Elongation at Yield 33.0 %ISO 527
Tensile Modulus 400 MPaISO 527
Flexural Modulus 400 MPaISO 178
Secant Modulus 0.0400 GPa
@Strain 50.0 %,
Temperature 120 °C
 0.0500 GPa
@Strain 50.0 %,
Temperature 100 °C
 0.0600 GPa
@Strain 50.0 %,
Temperature 80.0 °C
 0.0700 GPa
@Strain 50.0 %,
Temperature 60.0 °C
 0.0800 GPa
@Strain 50.0 %,
Temperature 40.0 °C
 0.0900 GPa
@Strain 50.0 %,
Temperature 23.0 °C
 0.100 GPa
@Strain 2.00 %,
Temperature 120 °C
 0.150 GPa
@Strain 2.00 %,
Temperature 100 °C
 0.200 GPa
@Strain 2.00 %,
Temperature 80.0 °C
 0.200 GPa
@Strain 25.0 %,
Temperature 0.000 °C
Yield
 0.250 GPa
@Strain 2.00 %,
Temperature 60.0 °C
 0.300 GPa
@Strain 2.00 %,
Temperature 40.0 °C
 0.300 GPa
@Strain 20.0 %,
Temperature -20.0 °C
Yield
 0.350 GPa
@Strain 2.00 %,
Temperature 23.0 °C
 0.750 GPa
@Strain 10.0 %,
Temperature -40.0 °C
Yield
 0.750 GPa
@Strain 1.00 %,
Temperature 0.000 °C
Yield
 1.25 GPa
@Strain 1.00 %,
Temperature -20.0 °C
Yield
 2.40 GPa
@Strain 0.000 %,
Temperature -40.0 °C
Yield
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 150 kJ/m²
@Temperature 23.0 °C
Type of failure: P; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+10 ohm-cmIEC 62631-3-1
Dielectric Constant 3.80
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 12.0
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 32.0 kV/mmAC, S20/P50; Sim. To IEC 60243-1
 37.0 kV/mmAC, S20/S20, t.; IEC 60243-1
Dissipation Factor 0.150
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 0.160
@Frequency 100 Hz
IEC 62631-2-1
Comparative Tracking Index 600 Vtest solution A, 50 drops value; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 170 µm/m-°C
@Temperature 25.0 - 55.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 160 µm/m-°C
@Temperature 25.0 - 55.0 °C
ISO 11359-1/-2
Melting Point 171 °CISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °CISO 75-1/-2
Vicat Softening Point 125 °C
@Load 5.10 kg
50 K/h; ISO 306
 165 °C
@Load 1.02 kg
50 K/h; ISO 306
Flammability, UL94 HB
@Thickness 1.30 mm
IEC 60695-11-10
 HB
@Thickness 3.20 mm
IEC 60695-11-10
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 °CInjection Molding; ISO 294
 220 °C
Mold Temperature 60.0 °CInjection Molding; ISO 294
 60.0 °C
Injection Velocity 200 mm/secInjection Molding; ISO 294
Injection Pressure 70.0 MPaInjection Molding; ISO 294
 
Descriptive Properties
Blue water consumption25.9 kgISO 14040, 14044
ColorBlack
Global Warming Potential2.6 kg CO2 eq./kgsavings incl. bio. C. as compared to classical production, ISO 14040, 14044
 5.7 kg CO2 eq./kgexcl. bio. C incl. LUC, ISO 14040, 14044
 5.8kg CO2 eq./kgincl. bio. C incl. LUC, ISO 14040, 14044
Land use (ReCiPe 2016)0.3 Annual crop eq. yISO 14040, 14044

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK7906 / 325038

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.