MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Mobil 1 0W-30
Categories: Fluid; Lubricant

Material Notes: Mobil 1 W-30 is an advanced high performance synthetic engine oil designed to provide outstanding wear protection and enhanced fuel economy performance. Mobil 1 0W-30 exceeds the requirements of the latest industry standards required by newer modern gasoline and certain diesel powered automobile engines. Mobil 1 technology is race proven and is the choice of race car drivers around the world. Mobil 1 0W-30 is perfect for all types of driving anywhere in the world and has the performance to protect where conventional engine oils do not.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.851 g/cc
@Temperature 15.0 °C
0.0307 lb/in³
@Temperature 59.0 °F
ASTM D4052
Viscosity 2.99 cP
@Temperature 150 °C
2.99 cP
@Temperature 302 °F
High Temperature High Shear (HTHS); ASTM D4683
Viscosity Measurement 175175Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 56 cSt56 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 10.3 cSt10.3 cStASTM D445
Ash 1.2 %1.2 %Sulfated Ash, wt%; ASTM D874
 
Thermal PropertiesMetricEnglishComments
Pour Point -54.0 °C-65.2 °FASTM D97
Flash Point 234 °C453 °FASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WEXXON018 / 75443

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.