MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Delrin Delrin® 577 BK000 POM-GF20
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, 20% Glass Fiber Reinforced

Material Notes: 20% Glass Filled Medium Viscosity Acetal Homopolymer

Information provided by DuPont; Delrin was sold by DuPont in 2023.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.56 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.017 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.011 cm/cmISO 294-4, 2577
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
cm³/10min Volumetric; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 52.0 MPaISO 527-1/-2
Elongation at Break 10 %ISO 527-1/-2
Tensile Modulus 4800 MPaISO 527-1/-2
Flexural Modulus 4600 MPaISO 178
Poissons Ratio 0.36
Charpy Impact, Notched 3.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 3.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 56.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 92.0 µm/m-°CISO 11359-1/-2
Melting Point 178 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 164 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 118 °CISO 75-1/-2
Flammability, UL94 HB
@Thickness 1.50 mm
IEC 60695-11-10
 HB
@Thickness 3.00 mm
IEC 60695-11-10
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 215 °COptimum, Injection
 210 - 220 °CRange, Injection
Mold Temperature 90.0 °COptimum, Injection
 80.0 - 100 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %Injection
Hold Pressure 80.0 - 100 MPaInjection
 100 MPaInjection
Annealing Temperature 160 °COptional; 2 mm/min; Injection
 
Descriptive Properties
AdditivesRelease agent
Annealing time (min/mm)30Optional, Injection
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Max. screw tangential speed (m/s)0.3Injection
Part Marking Code>POM-GF20<ISO 11469
PolymerPOM-GF20
Processing Hold Pressure Time (s/mm)8Injection
Resin IdentificationPOM-GF20ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Delrin Delrin® 570 NC000 POM-GF20
Delrin Delrin® 100STE NC010 POM-HI
Delrin Delrin® 525GR NC000 POM-GF25
Arkema Rilsamid® AZM 30 BLACK T6LD PA12-GF30
Celanese Celcon® GC25T POM, 25% Glass Reinforced

PDSX5138 / 197778

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.