MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECAPRO™ SAN Polypropylene (PP)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: TECAFORM™ (Polyacetal) and TECAPRO™ SAN (Polypropylene), provide an additional safety factor in reducing incidence of bacterial contamination. The raw materials are charged with an antimicrobial additive. These silver ions are released gradually to reduce the formation of bacterial.

  • Less bacterial contamination
  • Reduced odor and biofilm formation
  • Diminished formation of bacteria in equipment
  • Active components are harmless to humans
  • Scrubbing surface renews antimicrobial effect
  • FDA conformity of raw material, color pigments and antimicrobial additive

TECAFORM™ SAN and TECAPRO™ SAN are ideal where continual sanitary and anti bacterial conditions are a requirement. Excellent for components in food processing equipments, bottling and canning machines, water handling and filtration equipment. Door handles and buttons in public places would benefit from reduction in transfer of bacteria. TECAPRO™ SAN is especially effective in surgical instruments, trays, work surfaces and cutting boards in medical as well as food storage and preparation areas.

Information Provided by Ensinger Industries, Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.0332 lb/in³ASTM D792
Moisture Absorption at Equilibrium 0.050 %
@Temperature 22.8 °C
50% RH; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 14500 psiISO 2039/1,2
Tensile Strength, Yield 4785 psiASTM D638, DIN EN ISO 527
Elongation at Break >= 30 %ASTM D638, ISO 527
Flexural Modulus 270000 psiASTM D790, ISO 178
Izod Impact Resistance 0.328 ft-lb/in²ISO 180
 
Thermal PropertiesOriginal ValueComments
Melting Point 325 °FDIN 53 736
Maximum Service Temperature, Air 212 °FLong Term
 250 °FSort Term
Deflection Temperature at 1.8 MPa (264 psi) 187 °FISO - 75/A
Flammability, UL94 HB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ensinger TECAPRO™ MT Medical Grade Polypropylene (PP)
Ensinger TECASON™ S Polysulfone (PSU)
Overview of materials for Polypropylene, Extrusion Grade
316 Stainless Steel, annealed sheet
Overview of materials for Austenitic

PENSIN011 / 92828

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.