MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Alliance S-26L Sintered SmCo Magnet
Categories: Metal; Electronic/Magnetic Alloy; Nonferrous Metal; Cobalt Alloy

Material Notes: Samarium cobalt magnets were developed in the 1960’s and are still commonly used today because of their excellent very high temperature characteristics. SmCo5 and Sm2Co17 are the two main compositions of this material. They are slightly less powerful than NdFeB magnets, however they are extremely resistant to demagnetization and have the lowest reversible temperature coefficients of all magnets. Because of the high cobalt content, they are costly and their prices tend to be volatile. Plating is typically not required for corrosion protection, however in certain applications they are plated to limit chipping. Most common usage for these materials is in the aerospace and medical industries.

Information provided by Alliance LLC.

Key Words: Samarium Cobalt Permanent Magnet
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density >= 8.40 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 5000 psi
Modulus of Elasticity 17000 ksi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000860 ohm-cm
@Temperature 20.0 °C
Magnetic Coercive Force, Hc 6000 - 8000 Oe
 6200 - 9000 OeIntrinsic
Magnetic Remanence, Br 10000 - 10800 Gauss
Magnetic Maximum Energy Product, BH 24 - 28 MGOe
Curie Temperature 825 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.00 µm/m-°CParallel to M
 11.0 µm/m-°CPerpendicular to M
Maximum Service Temperature, Air <= 250 °CContinuous
 
Descriptive Properties
CompositionSm, Co, Cu, Zr, Pr
Required Magnetizing Force (Oe)35000
Reversible Temperature Coefficients-0.03α Br. %/°C
 -0.04β Hcj. %/°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NALLIAN56r / 268386

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.