MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Techmer ES HiFill® PP GB30 30% Glass Beads Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Glass Bead Filled

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Glass Bead, 30% Filler by Weight

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccASTM D792
Water Absorption 0.020 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.017 in/in
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 97ASTM D785
Tensile Strength, Yield 3400 psiASTM D638
Elongation at Yield 9.0 %ASTM D638
Flexural Yield Strength 4700 psiASTM D790
Flexural Modulus 270000 psiASTM D790
Izod Impact, Notched 0.600 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Strength 500 V/milMethod A (Short-Time); ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 36.0 µin/in-°FASTM D696
Melting Point 338 °F
Deflection Temperature at 0.46 MPa (66 psi) 240 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 155 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 100 GB 30 Polypropylene (PP), Glass Bead
A. Schulman POLYFORT™ FXP 3000-3120 Glass Sphere Filled Copolymer Polypropylene
Celanese SO.F.TER Polifor® 8 GB/30 30% Glass Bead Reinforced Polypropylene
Plastcom SLOVALEN PH 61 GB 30 PP, 30% glass beads, mod. of mech. prop.
Nurel Engineering Polymers Promyde® B30 P2 GB30 PA 6, Dry, 30% Glass Spheres Reinforced, Injection Molded and Heat Stabilized

PTPC0555 / 136493

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.