MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kraton® Kraton® G-2706 Styrene-based Biomedical Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.900 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 28ASTM D2240
Tensile Strength, Ultimate 850 psiASTM D412
Tensile Strength, Yield 0.130 ksiat 100%; ASTM D412
Elongation at Break 950 %ASTM D412
Tear Strength 140 plidie B; ASTM D624

References for this datasheet.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Advanced Elastomer Systems Santoprene® 8281-35W237 Thermoplastic Rubber
Dow Silastic® MDX4-4210 BIOMEDICAL GRADE ELASTOMER WITH CATALYST
Kraton® Kraton® D-2103 Styrene-based Biomedical Elastomer
Kraton® Kraton® G-2701 Styrene-based Biomedical Elastomer
NuSil MED-1000 Silicone, One Part Adhesive/Sealant - Restricted Medical Use

PMEDID29 / 52689

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.