MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NatureWorks® Ingeo™ 7001D ISBM Bottle Grade Biopolymer
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Ingeo biopolymer 7001D is a thermoplastic resin derived from annually renewable resources and is specifically designed for use in injection stretch blow molded (ISBM) bottle applications. Ingeo biopolymer 7001D can be run using conventional ISBM equipment, but processes at lower temperatures than PET and can attain good resolution of mold detail on conventional tooling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccASTM D1505
Moisture Vapor Transmission 13.8 - 15.7 cc-mm/m²-24hr-atmASTM F1249
Oxygen Transmission 25.6 - 27.6 cc-mm/m²-24hr-atmASTM D3985
Carbon Dioxide Transmission 106 - 118 cc-mm/m²-24hr-atmNatureWorks test
Viscosity Measurement 4.0
@Temperature 30.0 °C
Relative viscosity; 1.0 g/dl chloroform
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 210 °C
 
Thermal PropertiesOriginal ValueComments
Melting Point 145 - 160 °CASTM D3418
Glass Transition Temp, Tg 55.0 - 60.0 °CASTM D3418
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %Transparent; thickness not specified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NatureWorks® Ingeo™ 6252D Meltblown Fiber Grade Biopolymer
Corbion Purac Blend A High Heat Homopolymer PLA
BASF Ecovio® C2224 F Blend Biodegradable Polyester
NatureWorks® Ingeo™ 6060D Fiber Grade PLA
NatureWorks® Ingeo™ 6201D Fiber Grade PLA

PNATU89d / 135572

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.