MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Elastosil® R 570/50 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Electrically conductive silicone rubber for press molding, which are peroxide curing.

Properties: ELASTOSIL® R 570/50 is not suitable for vulcanization using crosslinker E. The materials are black.

Special features:

  • good mechanical and electrical properties
  • high conductivity
  • low volume resistivity
  • good heat resistance
  • good rheological properties
  • combustion products of low toxicity and corrosivity and low smoke density
Application: Control elements for cable accessories, contacts and keypads, interconnectors, electrically conductive rollers, electrodes.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccDIN 53479
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 49DIN 53505
Tensile Strength at Break 6.70 MPaDIN 53504 S1
Elongation at Break 370 %DIN 53504 S1
Tear Strength 16.0 kN/mASTM D624 B
Compression Set 37 %
@Temperature 175 °C,
Time 79200 sec
DIN ISO 815-B
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 7.4 ohm-cmDIN IEC 93
 
Descriptive Properties
Appearanceblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
Wacker Elastosil® R plus 573/50 A/B Silicone Rubber
Elkem (Bluestar Silicones) BLUESIL™ RTV 1556 B Silicone Rubber

PWACK9222 / 204751

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.