MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Indium Corp. Indalloy® 183 Au-Ge Solder Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Gold Alloy; Solder/Braze Alloy

Material Notes: Eutectic die attach.

Information Provided by Indium Corporation

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 14.67 g/cc0.5300 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 185 MPa26800 psi
Modulus of Elasticity 72.74 GPa10550 ksi
Shear Strength 185 MPa26800 psiShear Bond Holding Strength
 
Thermal PropertiesMetricEnglishComments
CTE, linear 13.0 µm/m-°C
@Temperature 20.0 °C
7.22 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 44.0 W/m-K
@Temperature 85.0 °C
305 BTU-in/hr-ft²-°F
@Temperature 185 °F
Melting Point 356 °C673 °FEutectic
Solidus 356 °C673 °F
Liquidus 356 °C673 °F
 
Component Elements PropertiesMetricEnglishComments
Germanium, Ge 12 %12 %
Gold, Au 88 %88 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Indium Corp. Indalloy® 182 Au-Sn Solder Alloy
Indium Corp. Indalloy 184 Gold Solder Alloy
Indium Corp. Indalloy® 263 Tin-Silver-Copper Solder Alloy
Indium Corp. Indalloy® 238 Sn-Au Solder Alloy
Epoxy Technology EPO-TEK® H20F Electrically Conductive, Flexible Epoxy

NNIN49 / 18505

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.