MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Rigid Extrusion L0189 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high water content only. This statement is only an overview of the FDA listings for this product. It is the customer's responsibility to ensure that the compound is suitable for its intended application.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.33 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 8415 sec; ASTM D2240
Tensile Strength, Yield 50.1 MPaType I, 5.1 mm/min; ASTM D638
Tensile Modulus 2700 MPaType I, 5.1 mm/min; ASTM D638
Flexural Strength 82.7 MPaASTM D790
Flexural Modulus 2680 MPaASTM D790
Izod Impact, Notched 110 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Compression Molded, Across Flow; ASTM D256A
 430 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Compression Molded, Flow; ASTM D256A
 1200 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
Dart Drop Total Energy 67.6 J/cm
@Temperature 23.0 °C
Procedure A, C.125; ASTM D4226
 178 J/cm
@Temperature 23.0 °C
Procedure B, C.125; ASTM D4226
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 74.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 67.8 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 182 - 193 °C
 
Compliance PropertiesOriginal ValueComments
FDA YesFood Contact, Unspecified Rating
 
Descriptive Properties
AppearanceClear/Transparent
FeaturesFood Contact Acceptable
FormsPellets
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Processing MethodExtrusion
PVC Cell Classification16443ASTM D1784
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesPiping
 Profiles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Geon® Performance Solutions HC 2195G Polyvinyl Chloride, Flexible
Formosa Plastics Formolon® 690 PVC
Formosa Plastics Formolon® 685 PVC
Formosa Plastics Formolon® 680H PVC
Denka VINYKON R2001 PVC, R grade for hard extrusion

PH0POL0562 / 145131

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.