MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eurofoam Porocell POR 304 B EPDM Foam
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.

Information provided by Eurofoam s.r.l.

Key Words: Referring Standard RE 42 / 2A2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.110 - 0.150 g/ccISO 845-88
Water Absorption <= 3.0 %ASTM D 1056
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 50 - 60ASTM D 2240
Tensile Strength 0.600 MPaASTM D 412
Elongation at Break >= 120 %ASTM D 412
Compressive Yield Strength 0.0420 MPa
@Strain 25 %
ASTM 1056/85
Tear Strength 0.450 kN/mASTM D 624
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 100 °CASTM D 3575
Minimum Service Temperature, Air -20.0 °CASTM D 3575
Shrinkage <= 4.0 %
@Temperature 70.0 °C,
Time 605000 sec
Linear; ASTM D 1204
 
Descriptive Properties
Cellular StructureClosed
ColorBlack
Declaration of Heavy Metal AbsenceConformRoHS2002/95/EC
Fire ResistanceMV22 302Pass
VulcanizationSulfur

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eurofoam Porocell POR 304 F-7142 EPDM Foam
Eurofoam Porocell POR 304 CM-GR EPDM Foam
Eurofoam Porocell POR 304 CM-HD 200 EPDM Foam
Eurofoam Porocell POR 304 CM-RS EPDM Foam
Eurofoam Porocell POR 304 CM-HD EPDM Foam

PEUROF912 / 157175

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.