MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 1199 X 117594 A Polyethylene Terephthalate (PET) Glass Fiber - Flame Retardant - Halogen Free
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.49 g/ccASTM D 792
Additive Loading 20 %Primary Additive
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
@Thickness 3.20 mm
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 11400 psiASTM D 638
Elongation at Break 1.2 - 1.5 %ASTM D 638
Tensile Modulus 1370 ksiASTM D 638
Flexural Strength 17400 psiASTM D 790
Flexural Modulus 1250 ksiASTM D 790
Izod Impact, Notched 1.40 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched 4.80 ft-lb/in
@Thickness 3.20 mm
ASTM D 4812
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-0
@Thickness 0.800 mm
 
Processing PropertiesOriginal ValueComments
Mold Temperature 275 - 300 °F
Drying Temperature 250 °F
@Time 14400 sec
Moisture Content 0.010 %
Dew Point -40.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 1199 A X 136859 B EG Polyethylene Terephthalate Glycol Modified (PETG); Permanently Static Dissipative - Extrusion Grade - ESD Protection
RTP Company RTP 1199 X 115085 E Polyethylene Terephthalate Glycol Modified (PETG), Carbon Nanotube - ESD Protection
RTP Company RTP 1199 X 115085 D Polyethylene Terephthalate Glycol Modified (PETG), Carbon Nanotube - ESD Protection
Eurotec® Tecopet® PT74 GR20 BK002 XA20 PET, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, black
Eurotec® Tecopet® PT70 GR15 NL100 PS20 PET, 15% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural, fast crystallization grade

PQZVA11864 / 120470

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.