MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik TEGOPREN® 5847 Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product description: TEGOPREN® 5847 is a polyether siloxane. It is a non-ionic product with 100 % active content.

Application: Apart from its extraordinary reduction of surface tension in aqueous solutions, the main property of TEGOPREN® 5847 is super spreading. This is the fast coverage of large hydrophobic surface. TEGOPREN® 5847 shows excellent surface wetting in adhesive application, where the coating of difficult substrates is required. Furthermore, it is recommended for curtain coating applications. The improvement of penetration into paper or its wetting of fibres, make TEGOPREN® 5847 suitable for adhesives used in the paper, wood and furniture market as well as for non-wovens and hygiene products.

Benefits: TEGOPREN® 5847 is a solvent-free easy to handle liquid. Due to its non-ionic nature it is compatible with cationic, anionic, non-ionic and amphoteric surfactants. The use of small amounts of TEGOPREN® 5847 reduces the surface tension of water-based systems. It therefore enhances the spreading on non-polare surfaces e. g. polypropylene.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 - 1.05 g/cc
Viscosity 50 - 100 cP
Surface Tension 23 dynes/cm0.1% in water
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 65.0 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.449 - 1.453
 
Descriptive Properties
AppearanceLiquid, colorless to pale brownish straw
Cloud point51-58°C4% solution

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik TEGOPREN® 5852 Additive
Evonik TEGOPREN® 5885 Additive
Evonik TEGO® Antifoam 2290 Antifoam concentrate
Evonik TEGOPREN® 5863 Defoamer
Evonik TEGOPREN® 5851 Defoamer

PEVONIL594 / 196798

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.