MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hyosung Topilene J340F PP
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: Topilene® J340F is a specially designed polypropylene block copolymer that features very high impact strength and excellent optical properties. It is suitable for retort CPP film extrusion. Topilene® J340F complies with FDA21 CFR 177.1520 and EU No 10/2011 for food contact.

Typical Applications: Retort CPP film/ Cast Film

Features: High Stiffness / High Impact Strength/Excellent Heat Resistance/ Low Fisheye / Good Heat Seal Strength

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D792
Melt Flow 2.6 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
Storage Temperature 40.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 90ASTM D785
Tensile Strength, Yield 300 kg(f)/cm²ASTM D638
Flexural Modulus 14000 kg(f)/cm²ASTM D790
Izod Impact, Unnotched 9.00 kg-cm/cmASTM D256
 4.00 kg-cm/cm
@Temperature -10.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 105 °CASTM D648
Vicat Softening Point 150 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 47 %40? CPP film; ASTM D1003
 
Processing PropertiesOriginal ValueComments
Drying Temperature 80.0 - 100 °C
Dry Time 2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hyosung Topilene J351F PP
Hyosung Topilene HJ340 PP
Hyosung Topilene HJ640A PP
Hyosung Topilene J800 PP
Hyosung Topilene HJ640 PP

PHYOS39 / 47925

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.