MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Biomer P304 PHB Biodegradable Polymer
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP

Material Notes: PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. PHB is waterproof and is highly crystalline (60 to 70%), providing excellent resistance to solvents.

PHB is a biopolymer which is present in all living organisms. Many bacteria produce PHB in large quantities as storage material (instead of fat, oil, or starch). It is not toxic and it is totally biodegradable. Biomer produces PHB and processes it to pellets that can be handled on plastics machines the same way as classic plastics produced from oil.

PHB is a biological storage material that is used by bacteria and fungi as feed source. The same is true for articles made of Biomer resins: they act as food supply to microorganisms and thus are biodegraded. PHB serves as nutrient only, when phosphates, nitrogen, salts, humidity, and heat allow the microorganisms to grow. Such conditions are present in composts and, in part, in the soil, but not under the conditions of typical use of injection molded or extruded articles. Therefore articles made of PHB stay unharmed for years.

Information provided by Biomer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/cc
Linear Mold Shrinkage 0.013 cm/cm
Deformation 2.5 %at bending break
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 69
Tensile Strength, Ultimate 25.0 - 28.0 MPa
Elongation at Break 8 - 15 %
Modulus of Elasticity 1.30 - 1.50 GPa
Flexural Strength 31.0 MPa
Charpy Impact Unnotched 5.00 - 6.00 J/cm²ISO 179/1eU
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 120 °C
Deflection Temperature at 1.8 MPa (264 psi) 80.0 - 100 °CISO 75/A
Vicat Softening Point 150 °C
Minimum Service Temperature, Air -30.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Goodfellow Polyhydroxybutyrate - Biopolymer PHB
Biomer P209 PHB Biodegradable Polymer
Goodfellow Polyhydroxybutyrate/Polyhydroxyvalerate (PHB 88/PHV 12)
Goodfellow Polyhydroxybutyrate / Polyhydroxyvalerate (PHB 92/PHV 8)
Biomer P226 PHB Biodegradable Polymer

PBIO507 / 190887

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.