MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kolon SPESIN® KP212VO Flame Retardant PBT Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Flame Retardant

Material Notes: SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.

High heat stability, outstanding abrasion resistance, excellent electrical properties, good surface gloss, low water absorption, excellent chemical resistance, good processability

Information provided by US distributor, API-Kolon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccDIN 53479; ASTM D792
Water Absorption 0.060 %DIN 53475; ASTM D570
Linear Mold Shrinkage 0.018 - 0.026 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 119DIN 53505; ASTM D785
Tensile Strength, Ultimate 650 kg(f)/cm²DIN 53455; ASTM D638
Elongation at Break 30 %DIN 53455; ASTM D638
Flexural Yield Strength 1200 kg(f)/cm²DIN 53455; ASTM D790
Flexural Modulus 31000 kg(f)/cm²DIN 53452; ASTM D790
Izod Impact, Notched 4.00 kg-cm/cmDIN 53453; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.2
@Frequency 1e+6 Hz
ASTM D150/DIN 53483
Dielectric Strength 25.0 kV/mmASTM D149/DIN 53481
Arc Resistance 85 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°C
@Temperature 20.0 °C
DIN 53752; ASTM D696
Melting Point 224 °CDIN 53736; ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 165 °CDIN 53461; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °CDIN 53461; ASTM D648
Flammability, UL94 HB

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
Kolon SPESIN® KP213G30 Flame Retardant PBT Resin

PKOL063 / 48969

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.