MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Description

Polyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in.

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.950 g/ccASTM D792
Melt Flow 20 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 22.0 MPaASTM D638
Elongation at Break 100 %ASTM D638
Flexural Modulus 0.990 GPaASTM D790
Izod Impact, Notched 180 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °CASTM D648
UL RTI, Electrical 115 °C
@Thickness 0.762 mm
UL 94
Flammability, UL94 V-2
@Thickness 1.57 mm
 V-2
@Thickness 3.05 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman POLYAXIS® PD2000 Polypropylene
BASF Capron® GR630 HS 30% Glass-Filled Nylon 66 (Dry)
Ensinger RADEL® R-5500 Polyphenylsulfone (PPSU)
Overview of materials for Polypropylene, Molded
A. Schulman POLYAXIS® PD8020 Polypropylene

PASHU096 / 25060

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.