MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® A3W2G10 BK 20560 50% Glass Filled PA66 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes: Description: 50% glass fiber reinforced injection molding grade with optimized heat ageing performance for industrial articles having very high rigidity.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.500 - 0.800 g/cc
Density 1.55 g/ccISO 1183
Water Absorption 3.7 - 4.3 %ISO 62
Moisture Absorption at Equilibrium 1.0 - 1.4 %ISO 62
Viscosity Measurement 140ISO 307
Linear Mold Shrinkage 0.0035 cm/cm
Linear Mold Shrinkage, Flow 0.0030 cm/cmISO 2577
Linear Mold Shrinkage, Transverse 0.0085 cm/cmISO 2577
Melt Flow 15.5 g/10 min
@Load 5.00 kg,
Temperature 275 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 255 MPaISO 527-1/-2
Elongation at Break 2.8 %ISO 527-1/-2
Modulus of Elasticity 16.0 GPaISO 527-1/-2
Charpy Impact Unnotched 100 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CISO 11357-1/-3
Maximum Service Temperature, Air 240 °C
Deflection Temperature at 0.46 MPa (66 psi) 250 °CISO 527-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 250 °CISO 527-1/-2
Decomposition Temperature >= 310 °C
Flammability, UL94 HB
@Thickness 1.60 mm
Ignition Temperature >= 400 °CASTM D1929
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 °CHopper Throat
Zone 1 300 °CFeed zone
Zone 2 300 °CCompression
Zone 3 300 °CMetering-zone
Zone 4 300 °CNozzle
Melt Temperature 280 - 310 °CInjection Molding/Extrusion
 300 °COptimal
Mold Temperature 80.0 °COptimal
 80.0 - 90.0 °CInjection Molding
Drying Temperature 80.0 °C
Dry Time 4 hour
Moisture Content 0.030 - 0.060 %Optimal
 <= 0.15 %
 
Descriptive Properties
ColorBK 20560
Commercial StatusEurope
Peripheral Screw Speed< 0.3 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® A3WG6 30% Glass Filled PA66 (Dry)
BASF Ultramid® A3W2G10 BK 20560 50% Glass Filled PA66 (Conditioned)
Aluminum 3003-H112
BASF Ultramid® A3HG6 HR BK 23591 30% Glass Filled PA66 (Conditioned)
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Dry)

PBASG0365 / 131998

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.