MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Iran Petrochemical (PCC) LF0200 Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Blow Molding Grade; Low Density Polyethylene (LDPE), Film Grade

Material Notes: LF0200 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties. LF0200 contains antioxidant.

Applications: general purpose bags, packaging of mechanical parts, industrial film, carrier bags, large bottles, coextruded milk bags, low tension power cable insulation, and industrial injection moldings.

Information provided by Iran Petrochemical Commercial Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/ccTSTM 209 B
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break >= 330 %ASTM D882, MD
 >= 600 %ASTM D882, TD
Dart Drop Test 100 gASTM D1709
Film Tensile Strength at Break, MD 15.7 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Softening Point 94.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 15 %ASTM D1003A
Gloss 60 %ASTM D523
 
Processing PropertiesOriginal ValueComments
Melt Temperature 160 - 180 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) LF0250/KJ Low Density Polyethylene
Iran Petrochemical (PCC) LF0190 Low Density Polyethylene
Iran Petrochemical (PCC) HB0035 High Density Polyethylene
Iran Petrochemical (PCC) 2100TN00 Low Density Polyethylene
Iran Petrochemical (PCC) 2102TX00 Low Density Polyethylene

PIPC248 / 149710

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.