MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik REWPAL® EO 70 Preparation agent
Categories: Fluid

Material Notes: Product description: Oleic acid polyglycol ester

Application: REWOPAL® EO 70 is used as a preparation agent and slickener for the preparation and processing of man made fibers. It is especially recommended as an oiling agent for synthetic fibers, wool and their blends. It can be used as a preparation agent on the backwashing machine or as an oiling agent for spinning and webbing mills. REWOPAL® EO 70 is recommended as dispersing agent for polyester oligomers in the reductive post-treatment bath at polyester dyeing. It can also be used as an emulsifier in mineral oil or ester based winding oils. Finally REWOPAL® EO 70 could be used as an additive in softener formulations for dyed goods to improve the hydrophilicity of the treated fabrics and fibers including mineral wool.

Properties / Benefits: REWOPAL® EO 70 is compatible with anionic, cationic, non-ionic and amphoteric surfactants. It is dispersible in water and could be diluted with demineralised water up to a sprayable 15 % concentrate. REWOPAL® EO 70 is clear soluble in mineral and ester oils and could also be used as emulsifier for these oils. REWOPAL® EO 70 added to softener formulations could increase the rewetting and water absorption of the treated fabric. Depending on the drying conditions REWOPAL® EO 70 could cause yellowing on white goods and needs therefore to be evaluated in the specific formulation and under the specific application conditions.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 6.5 - 7.56.5 - 7.5
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 6.0<= 6.0
 
Descriptive Properties
Appearanceyellow, clear liquid
Content89-95 mg KOH/gEster

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Green Glass Paper Thermal Ceramic
Pyrotek U-1 Compressible Board
Thermal Ceramics FireMaster Marine Blanket
Thermal Ceramics V-19 Block Insulation
Evonik BREAK-THRU® DA 646 Surfactants

PEVONIL510 / 196714

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.