MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Medalist® MD-53253 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Medalist MD-53200 series is a high performance thermoplastic elastomer series, designed to be a sustainable alternative to flexible PVC for medical tubing and film. Medalist MD-53253 is a medium hardness, low density, clear grade, available in Nat and color-matched, intended for use in medical and healthcare applications, with excellent processability and throughput in extruded tubing.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Autoclave Sterilizable; Chemical Resistant; Ethylene Oxide Sterilizable; Good Adhesion; Good Processability; Good Sterilizability; halogen Free; High Clarity; Medium Hardness; High Purity; Low Density; Low Specific Gravity; No Animal Derived Components; Radiation (Gamma) Resistant

Uses: Clear Sheet; Film; Hose; Medical/Healthcare Applications; Pharmaceuticals; Rubber Replacement; Tubing

Agency Ratings: ISO 10993 Part 5; ISO 13485

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Cast Film; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.890 g/ccASTM D792
Melt Flow 3.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 53
@Time 5.00 sec
ASTM D2240
 55
@Time 1.00 sec
ASTM D2240
Tensile Strength at Break 1650 psiDie C, 20 in/min; ASTM D412
Tensile Stress at Strain 190 psi
@Strain 50 %
Die C, 20 in/min; ASTM D412
 230 psi
@Strain 100 %
Die C, 20 in/min; ASTM D412
 400 psi
@Strain 300 %
Die C, 20 in/min; ASTM D412
Elongation at Break 670 %Die C, 20 in/min; ASTM D412
Tear Strength 165 pliDie C, 20 in/min; ASTM D624
Compression Set 13 %
@Temperature 22.8 °C,
Time 79200 sec
Type 1; ASTM D395
 100 %
@Temperature 70.0 °C,
Time 79200 sec
Type 1; ASTM D395
 
Processing PropertiesOriginal ValueComments
Zone 1 320 - 370 °F
Zone 2 360 - 385 °F
Zone 3 360 - 400 °F
Zone 4 360 - 400 °F
Zone 5 360 - 410 °F
Die Temperature 350 - 420 °F
Screw Speed 30 - 100 rpm
 
Descriptive Properties
AppearanceClear/Transparent
 Colors Available

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals NI-SPAN-C® Alloy 902
Silberline SilBerCote® PC 1291X
Mocom (ALBIS) ALTECH® PC+ABS ECO 1000/500 PC+ABS
Covestro Bayblend® FR3210 TV PC/ABS Blend
Aluminum, Al

PTEKNQ0743 / 237234

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.