System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Mocom (ALBIS) Altech® NXT PP PP-B A 2035/450 GF35 CP 35% Glass Filled PP Copolymer
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene with 40% Glass Fiber Filler
Material Notes:
Polypropylene Heterophasic Copolymer, 35% glass fibers. Chemically coupled, high heat stabilized, high stiffness, high toughness. Applications: automotive, various. Pre drying conditions unnecessary
Information provided by ALBIS.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.17
g/cc
ISO 1183
Linear Mold Shrinkage
0.0010
-
0.0040
cm/cm
@Time 86400 sec
ISO 294-4
0.0020
-
0.0060
cm/cm
@Time 86400 sec
ISO 294-4
Spiral Flow
30.0
cm
@Thickness 1.00 mm
80.0
cm
@Thickness 2.00 mm
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
66.0
MPa
ISO 527-1/-2
Elongation at Break
3.7 %
ISO 527-1/-2
Tensile Modulus
6400
MPa
ISO 527-1/-2
Flexural Strength
105
MPa
ISO 178
Flexural Modulus
5500
MPa
ISO 178
Charpy Impact Unnotched
50.0
kJ/m²
ISO 179/1eU
50.0
kJ/m²
@Temperature -40.0 °C
ISO 179/1eU
Charpy Impact, Notched
15.0
kJ/m²
ISO 179/1eA
10.0
kJ/m²
@Temperature -40.0 °C
ISO 179/1eA
Thermal Properties
Original Value
Comments
Melting Point
168
°C
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi)
150
°C
ISO 75-1/-2
Vicat Softening Point
105
°C
B50; ISO 306
Flammability, UL94
HB
@Thickness 1.50 mm
Processing Properties
Original Value
Comments
Melt Temperature
200
-
270
°C
injection molding
Mold Temperature
20.0
-
90.0
°C
injection molding
Drying Temperature
80.0
°C
@Time 7200 - 10800 sec
for superior surface quality
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Mocom (ALBIS) Altech® NXT PP PP-H A 2040/456.01 LE GF40 CP 40% Glass Filled PP Homopolymer
Borealis Xmod™ K65G3 30% Glass Fiber Reinforced Polypropylene Compound
Borealis Xmod™ GD301HP High Performance 32% Glass Fiber Reinforced
Bamberger Polymers Bapolene® 4012F Polypropylene, Compounding/Extrusion Grade
Avient Maxxam™ XN-418.G001-1000 Polypropylene Copolymer (PP Copolymer)
PALBIS9916 / 221012
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.