MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese SO.F.TER Polifor® E 8 TR/30 Elastomer Modified Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:

Information provided by SO.F.TER. Spa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccASTM D1505
Linear Mold Shrinkage 0.012 - 0.015 cm/cmASTM D955
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 23.0 MPaASTM D638
Elongation at Break 50 %ASTM D638
Flexural Modulus 1900 MPaASTM D790
Izod Impact, Notched 120 J/mASTM D256/A
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index >= 600 VIEC 112
 
Thermal PropertiesOriginal ValueComments
Hot Ball Pressure Test >= 115 °CIEC 335
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °CASTM D648
Vicat Softening Point 57.0 °C50°C/h at 50 N; ASTM D1525
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 3.20 mm
Oxygen Index 21 %ASTM D2863
Glow Wire Flammability Index 650 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 190 - 230 °CCylinder Temperature
Mold Temperature 40.0 - 60.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis HD905CF Polypropylene Homopolymer for Cast Film
Borealis Daplen™ ED206HP TPO Compound
Formosa Plastics Formolene® 5144L Homopolymer Polypropylene
Ineos H07B-01 Polypropylene Homopolymer
LyondellBasell Adstif HA 748L Polypropylene

PSOFS798 / 162262

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.