MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ametek AM 388™ Alloy (UNS C72650) TB00 Solution HT
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Information supplied by Ametek Specialty Metal Products Division.

Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and switches.

Benefits include combination of high strength and formability, high conductivity, available in mill hardened or age hardenable tempers, no distortion during aging, no fixturing required, excellent solderability and resistance to stress relaxation during high temperature (over 400°F, 200°C) soldering, fine grain size, excellent corrosion resistance bare and easy to plate when required, low initial cost, and additional savings during processing.

Aging Temperature/Time 725°F-750°F (385°C-400°C)/1.5-3 hrs.

Key Words: Copper Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.87 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 100 - 130
Tensile Strength, Ultimate 379 - 482 MPa
Tensile Strength, Yield 172 - 241 MPa
@Strain 0.2 %
Elongation at Break 32 - 40 %typical
Modulus of Elasticity 124 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000011 - 0.000012 ohm-cm14 - 15% IACS
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 87 %as balance
Nickel, Ni 7.0 - 8.0 %
Other <= 0.50 %
Tin, Sn 4.5 - 5.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Brush Wellman Beryllium Copper Alloy 165 Strip; A-Dead soft (TB00) Temper (UNS C17000)
Brush Wellman Beryllium Copper Alloy 165 Strip; 1/4H (TD01) Temper (UNS C17000)

NMA255 / 18174

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.