MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Makrolon® LQ3187 Optical Grade Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Optical Grade

Material Notes: MVR (300 °C/1.2 kg) 6.0 cm³/10 min; optical lens; high viscosity; UV stabilized; UV 400 cut off; easy release; injection molding - melt temperature 280 - 320 °C; safety glasses; sun glasses

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.660 g/ccpellets; ISO 60
Density 1.20 g/ccISO 1183
Moisture Absorption at Equilibrium 0.12 %ISO 62
Water Absorption at Saturation 0.30 %ISO 62
Water Vapor Transmission 15.0 g/m²/day
@Thickness 0.100 mm,
Temperature 23.0 °C
85% RH; ISO 15106-1
Oxygen Transmission 650 cc-mm/m²-24hr-atmcm³/(m²·24 h·bar), 100 µm film; b.o. ISO 2556
 2760 cc-mm/m²-24hr-atmcm³/(m²·24 h·bar), 25.4 µm (1 mil) film; b.o. ISO 2556
Nitrogen Transmission 120 cc-mm/m²-24hr-atmcm³/(m²·24 h·bar), 100 µm film; b.o. ISO 2556
 510 cc-mm/m²-24hr-atmcm³/(m²·24 h·bar), 25.4 µm (1 mil) film; b.o. ISO 2556
Carbon Dioxide Transmission 3800 cc-mm/m²-24hr-atmcm³/(m²·24 h·bar), 100 µm film; b.o. ISO 2556
 16900 cc-mm/m²-24hr-atmcm³/(m²·24 h·bar), 25.4 µm (1 mil) film; b.o. ISO 2556
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cmparallel/normal; b.o. ISO 2577
Linear Mold Shrinkage, Flow 0.0070 cm/cm60x60x2 mm; 500 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0075 cm/cm60x60x2 mm; 500 bar; ISO 294-4
Melt Flow 6.5 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 116 MPaISO 2039-1
Tensile Strength at Break 70.0 MPa50 mm/min; ISO 527-1/-2
Tensile Strength, Yield 66.0 MPa50 mm/min; ISO 527-1/-2
Elongation at Break >= 50 %Nominal, 50 mm/min; ISO 527-1/-2
 120 %50 mm/min; ISO 527-1/-2
Elongation at Yield 6.2 %50 mm/min; ISO 527-1/-2
Tensile Modulus 2400 MPa1 mm/min; ISO 527-1/-2
Flexural Strength 98.0 MPa2 mm/min; ISO 178
Flexural Yield Strength 74.0 MPa
@Strain 3.5 %
2 mm/min; ISO 178
Flexural Modulus 2.40 GPa2 mm/min; ISO 178
Flexural Strain at Yield 7.0 %2 mm/min; ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²
@Thickness 3.00 mm,
Temperature -30.0 °C
complete break; ISO 7391/b.o. ISO 180-A
 70.0 kJ/m²
@Thickness 3.00 mm,
Temperature 23.0 °C
partial break; ISO 7391/b.o. ISO 180-A
Charpy Impact Unnotched NBISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
 NB
@Temperature -60.0 °C
ISO 179/1eU
Charpy Impact, Notched 1.40 J/cm²
@Thickness 3.00 mm,
Temperature -30.0 °C
complete break; ISO 7391/b.o. ISO 179-1eA
 8.00 J/cm²
@Thickness 3.00 mm,
Temperature 23.0 °C
partial break; ISO 7391/b.o. ISO 179-1eA
Impact 5600Puncture - maximum force (N); ISO 6603-2
 6500
@Temperature -30.0 °C
Puncture - maximum force (N); ISO 6603-2
Puncture Energy 60.0 JISO 6603-2
 70.0 J
@Temperature -30.0 °C
ISO 6603-2
Tensile Creep Modulus, 1 hour 2200 MPaISO 899-1
Tensile Creep Modulus, 1000 hours 1900 MPaISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohmIEC 60093
Dielectric Constant 3.0
@Frequency 1e+6 Hz
IEC 60250
 3.1
@Frequency 100 Hz
IEC 60250
Dielectric Strength 34.0 kV/mm1 mm; IEC 60243-1
Dissipation Factor 0.00050
@Frequency 100 Hz
IEC 60250
 0.0095
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 125 VCTI M; Solution B; IEC 60112
 250 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
Thermal Conductivity 0.200 W/m-Kcross-flow; ISO 8302
Hot Ball Pressure Test 137 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 137 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 125 °CISO 75-1/-2
Vicat Softening Point 146 °C50°C/h 50N; ISO 306
 147 °C120°C/h 50N; ISO 306
Glass Transition Temp, Tg 145 °CISO 11357-1/-2
Flash Point 480 °Cignition; ASTM D1929
 550 °Cself ignition; ASTM D1929
Oxygen Index 28 %Method A; ISO 4589-1/-2
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586Procedure A; ISO 489
Abbe Number 30
Haze 1.0 %
@Thickness 3.00 mm
ISO 14782
Transmission, Visible <= 85 %
@Thickness 4.00 mm
ISO 13468-2
 88 %
@Thickness 3.00 mm
ISO 13468-2
 89 %
@Thickness 1.00 mm
ISO 13468-2
 89 %
@Thickness 2.00 mm
ISO 13468-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 300 °CInjection Molding; ISO 294
Mold Temperature 80.0 °CInjection Molding; ISO 294
Injection Velocity 200 mm/secISO 294
 
Descriptive Properties
Electrolytic corrosionA1IEC 60426

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 5052-H32
Aluminum 6061-T6; 6061-T651
Covestro Makrolon® 1952 Polycarbonate
Covestro Makrolon® 2407 Polycarbonate, Injection Grade
Covestro Makrolon® 2558 Polycarbonate

PB09963 / 92803

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.