MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kumho-Sunny Ecoblend® PAE9730 Renewable/Recycled Polymer
Categories: Polymer; Renewable/Recycled Polymer

Material Notes: PAE9730 is general purpose resin. PAE9730 is mainly used in ornament of small appliance, shell & panel of PC box, etc.

Information provided by Shanghai Kumho Sunny Plastics co, Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccASTM D792
Maximum Moisture Content 0.020
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cmASTM D955
Melt Flow 15 g/10 min
@Load 5.00 kg,
Temperature 240 °C
ASTM D1238
 15 g/10 min
@Load 5.00 kg,
Temperature 265 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 50.0 MPaASTM D638
Elongation at Break 40 %ASTM D638
Flexural Strength 65.0 MPaASTM D790
Flexural Modulus 1850 MPaASTM D790
Izod Impact, Notched 400 J/m
@Thickness 3.20 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmICE 60093
Surface Resistance >= 1.00e+15 ohmICE 60093
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °CASTM D648
Vicat Softening Point 100 °CB; ASTM D1525
Flammability, UL94 HB
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 230 - 240 °C
Middle Barrel Temperature 250 - 260 °C
Front Barrel Temperature 265 - 275 °C
Nozzle Temperature 260 - 270 °C
Melt Temperature 265 - 275 °C
Mold Temperature 80.0 - 100 °C
Drying Temperature 80.0 - 90.0 °C
Dry Time 3.00 - 4.00 hour
Back Pressure 1.00 - 5.00 MPa
Screw Speed 40 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKMSN000 / 280852

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.