MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Makrolon® 3207 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: General purpose; high viscosity; UV stabilized; easy release; developed for safety goggles

Mechanical property data for samples at 50% RH.

Information provided by Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccISO 1183-1
Linear Mold Shrinkage 0.0073 in/in60x60x2 mm; ISO 294-4
Linear Mold Shrinkage, Flow 0.0073 in/in60x60x2 mm; ISO 294-4
Melt Flow 4.76 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 62.0 MPa50mm/min; ISO 527-1,-2
Elongation at Break >= 50 %5mm/min, complete break; ISO 524-1,-2
 68 %5mm/min, complete break; ISO 524-1,-2
Elongation at Yield 6.5 %50mm/min; ISO 527-1,-2
Tensile Modulus 2270 MPa
@Temperature 23.0 °C
1mm/min, complete break; ISO 527-1,-2
Flexural Strength 97.0 MPa2mm/min; ISO 178
 72.0 MPa
@Strain 3.5 %
2mm/min; ISO 178
Flexural Modulus 2400 MPa
@Temperature 23.0 °C
2mm/min; ISO 178
Flexural Strain at Break 7.5 %2 mm/min; ISO 178
Izod Impact, Notched (ISO) 20.0 kJ/m²
@Thickness 3.20 mm,
Temperature -30.0 °C
b.o. ISO 180-A
 71.0 kJ/m²
@Thickness 3.00 mm,
Temperature -20.0 °C
ISO 7391/b.o. ISO 180-A
 75.0 kJ/m²
@Thickness 3.00 mm,
Temperature 23.0 °C
Partial Break; ISO 7391/b.o. ISO 180-A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179-1eU
 NB
@Temperature -30.0 °C
ISO 179-1eU
 NB
@Temperature -60.0 °C
ISO 179-1eU
Puncture Energy 60.0 J
@Temperature 23.0 °C
complete break; ISO 6603-2
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 141 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 130 °CISO 75-1,-2
Vicat Softening Point 149 °C
@Load 5.10 kg
@ 50°C/h; ISO 306
 150 °C
@Load 5.10 kg
@ 120°C/h; ISO 306
Glass Transition Temp, Tg 151 °C10°C/min; ISO 11357-1,-2
 
Optical PropertiesOriginal ValueComments
Haze <= 0.20 %
@Thickness 3.00 mm
for transparent material; ISO 14782
Transmission, Visible 88 %
@Thickness 3.00 mm
Luminous; ISO 13468-2
 88 %
@Thickness 4.00 mm
Luminous; ISO 13468-2
 89 %
@Thickness 1.00 mm
Luminous; ISO 13468-2
 89 %
@Thickness 2.00 mm
Luminous; ISO 13468-2
 
Descriptive Properties
Puncture Maximum Force (N)5715ISO 6603-2, at 23°C, complete break

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® 2608 Polycarbonate
Covestro Makrolon® 6265X Polycarbonate
Covestro Makrolon® 2807 MAS 167 Polycarbonate
Covestro Makrolon® ET 3113 Polycarbonate
Teijin Panlite® L-1225 Polycarbonate, Standard Grade

PB095060 / 200130

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.