MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI Type 316N Stainless Steel, annealed sheet
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Nonhardenable, higher strength than conventional 316, yet retains ductility, as well as good corrosion and heat resistance. Nonmagnetic annealed, becomes slightly magnetic when cold worked. Good corrosion resistance to most chemicals, salts, and acids and molybdenum content helps resistance to marine environments. High creep strength at elevated temperatures. Fabrication characteristics similar to Types 302 and 304. Applications include chemical processing, food processing, photographic, pharmaceutical, textile finishing, marine exterior trim.

Key Words: UNS S31651, AISI 316N, ISO 4954 X6CrNiMoTi122E, ISO 683/13 21
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.92 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 85
Tensile Strength, Ultimate 620 MPa
Tensile Strength, Yield 330 MPa
Elongation at Break 48 %in 50 mm
Tensile Modulus 196 GPa
Izod Impact 80.0 J
@Diameter 13.0 mm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000740 ohm-cmat 20ºC
Magnetic Permeability 1.008at RT
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.0 µm/m-°C
@Temperature 0.000 - 100 °C
 16.2 µm/m-°C
@Temperature 0.000 - 315 °C
 17.5 µm/m-°C
@Temperature 0.000 - 540 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 16.1 W/m-K
@Temperature 95.0 °C
Melting Point 1370 - 1400 °C
Solidus 1370 °C
Liquidus 1400 °C
Maximum Service Temperature, Air 870 °CIntermittent
 925 °CContinuous Service
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.080 %
Chromium, Cr 16 - 18 %
Iron, Fe 61.69 - 71.9 %As Balance
Manganese, Mn <= 2.0 %
Molybdenum, Mo 2.0 - 3.0 %
Nickel, Ni 10 - 14 %
Nitrogen, N 0.10 - 0.16 %
Phosphorus, P <= 0.045 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 316N Cast Stainless Steel, ACI
Cast Stainless Steel CF3MN, ACI
AISI 316N Cast Stainless Steel, UNS J92804
Cast Stainless Steel CF3MN, ASTM A743
AISI Type 316LN Stainless Steel, Composition Spec

MQ316S / 12806

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.