HA104E is a natural high molecular weight, high melt flow rate polypropylene homopolymer characterized by well-balanced stiffness to impact strength ratio at increased processing properties. Applications HA104E is recommended for non-pressure pipes and fittings, structured wall pipes and profiles and sheets.Information provided by Borealis AG |