MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lucite International Perspex™ GS Acrylic Cast Sheet 000/0000
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Cast

Material Notes: PERSPEX cast sheet is made between sheets of high quality glass and produced in batches. It has a very high molecular weight making it strong, resilient and easy to handle and fabricate. The cast method of manufacture is ideally suited to small colour runs and batch sizes.

Information provided by Lucite International.

Key Words: PMMA; Polymethyl Methacrylate; Polymethylmethacrylate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccISO 1183
Water Absorption 0.20 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 102ISO 2039-2
Tensile Strength, Ultimate 75.0 MPa5 mm/min; ISO 527
Elongation at Break 4.0 %5 mm/min; ISO 527
Flexural Strength 116 MPa2 mm/min; ISO 178
Flexural Modulus 3.21 GPa2 mm/min; ISO 178
Charpy Impact Unnotched 1.20 J/cm²ISO 179
 
Thermal PropertiesOriginal ValueComments
CTE, linear 77.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Vicat Softening Point >= 110 °CISO 306A
Flammability, UL94 HB
Flammability Test 3.0BS 476, Pt7
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49ISO 489/A
Transmission, Visible >= 92 %clear grade; in 3 mm (colored grades lower); ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lucite International Perspex™ GS IM Acrylic Cast Sheet OM14
Overview of materials for Acrylic, Cast
Lucite International Perspex™ XT Acrylic Extruded Sheet 0X00
Lucite International Perspex™ XT IM50 Acrylic Extruded Sheet
Polycasa CAST PMMA

PLUCIT00 / 52053

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.