MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Elkem (Bluestar Silicones) SILBIONE® HCRA 4150 A/B HC Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: SILBIONE® HCRA 4150 A/B HC is a two-part, addition-cure, platinum catalyzed silicone elastomer designed for use in processes where high strength molded parts or extruded profiles are desired. It is formulated for rapid cure in transfer and compression molds and in short-dwell vulcanizing ovens for extrusion processes. SILBIONE ® HCRA 4150 A/B HC meets USP Class VI requirements and can be used in short term (under 30 days) implant materials.

Applications:

  • Molded or extruded medical parts for <30 day implantation
  • Healthcare applications: stoppers, plungers, seals, needle entry ports, tubing
Features:
  • No volatile cure by-products
  • Optional post cure
  • Non-tacky surface
  • Non-blooming
  • No peroxide residue

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/ccTP 013
Storage Temperature 24.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 50ASTM D2240
Tensile Strength 1600 psiASTM D412
Elongation at Break 700 %ASTM D412
Tear Strength 230 pliASTM D624, Die B
Tensile Set 3.0 %ASTM D412
 
Processing PropertiesOriginal ValueComments
Cure Time 0.167 hour
 10.0 min
@Temperature 120 °C
Post cure for 1 hr at 165°C
Pot Life 480 minNM 128
Shelf Life 6.00 Month
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
AppearanceClear, translucent solid
Mix Ratio1:1A:B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Elastosil® R plus 4000/50 Silicone Rubber
Rogers Arlon 10842S020 0.020" (0.508 mm) Fully Cured, Unsupported, Silicone Rubber
Precision Polymer Engineering S60R Silicone Rubber
NuSil MED-4755 Ultra High Performance High Consistency Elastomers - Unrestricted Medical Use
Multibase C6-135 Dow-Corning Class VI Elastomer

PBLUST082 / 191058

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.