MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexTow® IM6 Intermediate Modulus Carbon Fiber (12,000 Filaments)
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: Weight/length = 0.446 g/m.

HexTow™ IM6 carbon fiber is a continuous, high performance, intermediate modulus, PAN based fiber available in 12,000 (12K) filament count tows. The fiber has been surface treated and can be sized to improve its interlaminar shear properties, handling characteristics, and structural properties. HexTow® IM6 fiber has shear properties equivalent to those of standard AS type fibers. It is suggested for use in prepregging and filament winding.
The unique properties of HexTow® IM6 fiber, such as lower density (5% less than AS type), higher modulus (20% stiffer than AS type fibers), and good shear strength, allow structural designers to achieve both higher safety margins and lower weights for both stiffness and strength critical applications.

Information provided by Hexcel Corporation. Values are typical average lot properties.

Key Words: Carbon Fibres
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.76 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 5723 MPa
Elongation at Break 1.9 %
Tensile Modulus 279 GPaat chord 6000-1000

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexTow® AS4C 3K Standard Modulus Carbon Fiber (3000 Filaments)
Hexcel® IM9 Intermediate Modulus Carbon Fiber (12,000 Filaments)
Hexcel® UHM Carbon Fiber (12,000 Filaments)
Hexcel® HexTow® IM6 Carbon Fiber - Epoxy Composite
Hexcel® HexTow® IM7 12K Intermediate Modulus Carbon Fiber (12,000 Filaments)

EHECF8 / 3120

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.